Kwon, H., Perez, C., Kim, H. K., Asheghi, M., Park, W., & Goodson, K. E. (2021). Thermal Interface Enhancement via Inclusion of an Adhesive Layer Using Plasma-Enhanced Atomic Layer Deposition. ACS Applied Materials & Interfaces. https://doi.org/10.1021/acsami.0c19197